Amorphous Bars

Amorphous Bars

Amorohous bas & Amorphous Block Core – SUNBOW’s amorphous-SWAM & nanocrystalline-SWNA alloys are based on Fe, Si, B and with further additions of Nb and Cu, and produced by rapid solidification technology.

Product Introduction

 

Amorohous bas & Amorphous Block Core – SUNBOW's amorphous-SWAM & nanocrystalline-SWNA alloys are based on Fe, Si, B and with further additions of Nb and Cu, and produced by rapid solidification technology.

Composition metals melt in furnace under around 1500℃, and turn into liquid metal which pass through a narrow nozzle, and solidify at rate of 1million degree/s. Atoms have no enough time to reach microstructure-crystalline state and stay in amorphous state.

A subsequent heat treatment-annealing at around 500~600℃ transforms the initially amorphous microstructure into nanocrystalline state in which fine crystalline grains (average grain diameter of 10-40 nm) embedded in an amorphous residual phase.

Application:High-power (especial more than 50KW) reactors of solar or wind inverters.

power transformer, high speed motor (rotor & stator), welding machine, induction heating, medical equipment (X-ray & CT), inductor and reactor (EV/HEV/FCV-Bulk & Boost, solar & wind-inverter, automation-converter & UPS, military)

 

Feature & Benefit

 

>Thickness (24μm) - smaller eddy & loss

>Coercivity (2.4A/m) - smaller hysteresis loss

>High Frequency(≤20KHz) - wider working range

>Big Saturation Flux Density (1.56T)- smaller dimension and less weight

 

SWAM-TYPICAL DATA

Saturation flux density

1.56

T

Coercivity

2.4

A/m

Maximum permeability

200,000

 

Initial permeability

1,000

 

Curie temperature

410

℃

Crystallization temperature

535

℃

Saturation magnetostriction

20~30

ppm

Core loss (10KHz, 0.1T)

≤2.3

W/kg

Density

7.2

g/cm3

Electrical resistivity

1.3

μΩ.m

Thermal expansional

4.7

ppm/℃

Working temperature

-55~155

℃

Layer thickness

24

24μm

Material composition

Fe-80%,Si-9%,B-11%

 

 

product-768-687

product-544-433

product-716-600

 

Other sizes can be customized .

 

Sunbow covering a long product chain of soft magnetic material (amorphous & nanocrystalline), parts (core/rotor &stator/terminal/shunt/busbar), components (current transformer/current transducer/common mode choke/inductor/reactor /power transformer)

Benefitting from one of our great strength-versatility, SUNBOW has enough ability to fill various requirements from our customers all over the world and design and produce qualified products for them.

 

Our wide range of high-quality and cutting-edge soft magnetic materials, parts, components, finished products enable us to supply sufficient power to customers and partners in various field of electricity(current transformer), wind & solar energy (inverter), automation equipment (converter & UPS), EV (inductor & EMC), rail traffic (power transformer), telecommunication (current transducer), military(reactor), medical equipment, utility(water & electricity meter)etc.

 

FAQ:

 

1.Which countries you are selling to ?

We export our cores to Germany, Italy, France, UK, Turkey, Spain, Sweden, Poland, Czech, Slovakia, Korea, Thailand, Malaysia, Indonesia, Vietnam, USA, Columbia, Brazil, Australia etc.

 

2.What is your payment terms?

We accept TT and L/C.


Advantages

1.We produce amorphous and nanocrystalline ribbons as raw materials for cores, so we can adjust the formulation of raw materials according to application and performance requirements

2.more then 13 years experiences in magnetic cores manufacturing and exporting.

3.Various types magnetic materials available: Silion Steels, Nanocrystalline ribbon, Amorphous Ribbon, Mumetal

4.professional customized service,various types of cores ,give you the best solution

 

For additional information and immediate assistance with your requirements, designs and applications, please call 021-63306968

Or send email to :sales@sunbowgroup.com

 

our workshop

 

our workshop

 

our equipment

 

our equipment1

our equipment2

 

our testing

 

our testing1

our testing2

 

our certification

 

our certification

 

our production process

 

our production process

 

our exhibition

 

page-1200-1200

 

Hot Tags: amorphous bars, China amorphous bars manufacturers, suppliers, factory, amorphous transformer core, amorphous block core, Magnetic Cores, Amorphous Bars, stator core laminations, Amorphous Products

Send Inquiry

(0/10)

clearall