SUNBOW’ R&D and engineering department has rich experience in designing cores and components for the current measurement industry. SUNBOW always focused on studying and improving our own soft magnetic material and finally developed SWFNA-nanocrystalline (iron-based) alloy as the adequate solution for current transformer cores.

Product Introduction

 

SUNBOW' R&D and engineering department has rich experience in designing cores and components for the current measurement industry. SUNBOW always focused on studying and improving our own soft magnetic material and finally developed SWFNA-nanocrystalline (iron-based) alloy as the adequate solution for current transformer cores.

 

FEATURE

> High permeability

> Low Cost and Low Core Loss

> High Saturation Flux Density

> High Linearity, Low Temperature Dependence

 

BENEFIT

> Low Phase Error

> Low Amplitude Error

> Large Current Range and Small Dimension

> Constancy of Phase and Amplitude Error

 

HIGH-LIGHT

>> High Saturation Flux Density <<

smaller dimension and less weight than permalloy core

 

>> Low Core Loss <<

core loss lower than permalloy core

>> Linear and Low Temperature Dependence <<

working more stable and longer in wider

temperature range of -55~130℃

 

>> Low Cost & High Effect <<

cheaper and more effective than permalloy core

 

PERMEABILITY/SATURATION/LINEARITY

A typical hysteresis loop of nanocrystalline and permalloy indicates that:

SWFNA cores has much higher linearity of permeability in the almost whole loop;

SWFNA cores also keeps higher permeability (μ=20,000) than permalloy;

SWFNA cores' saturation (1.23T) is impressively higher than permalloy's (0.75T).

All above plus advantage of lower cost than permalloy makes SWFNA cores become excellent option for purpose of current transformer.

 

product-512-405

Fig.3 Typical hysteresis loop of SWFNA and permalloy

product-854-590

 

Part Code

SWFNA-CT

Mean

Path

Length

mm

Outer

Diameter

a/mm

Inner

Diameter

b/mm

Height

c/mm

Outer

Diameter

(casing)

A/mm

Inner

Diameter

(casing)

B/mm

Height

(casing)

C/mm

Cross

Section

Ac/mm2

64-T001 HP

64.40

18.0

13.0

5.0

20.0

10.0

7.5

10.0

65-T002 HP

65.97

19.0

15.0

6.5

22.5

12.0

9.0

10.4

73-T003 HP

73.87

21.0

16.0

10.0

23.8

14.5

12.5

20.0

91-T004 HP

91.11

25.0

17.0

8.0

27.0

15.0

10.0

25.6

103-T005 HP

103.67

29.0

21.0

6.5

31.0

19.0

8.4

20.8

109-T006 HP

109.96

30.0

20.0

8.0

33.0

17.5

10.5

32.0

135-T007 HP

135.87

39.1

30.8

6.5

41.0

29.5

8.4

21.6

207-T008 HP

207.35

60.0

48.0

15.0

63.0

45.0

18.0

72.0

201-T001 HV

201.6

55.0

37.0

20.0

60.0

32.0

25.0

144.0

400-T002 HV

400.55

115.0

90.0

10.0

120.0

85.0

15.0

100.0

911-T003 HV

911.06

260.0

200.0

35.0

265.0

195.0

41.0

840.0

997-T004 HV

997.46

280.0

205.0

90.0

285.0

200.0

97.0

2700.0

1256-T005 HV

1256.64

350.0

250.0

30.0

355.0

245.0

35.0

1200.0

1429-T006 HV

1429.42

390.0

260.0

25.0

395.0

255.0

30.0

1300.0

1555-T007 HV

1555.09

450.0

360.0

20.0

455.0

355.0

25.0

720.0

1586-T008 HV

1586.50

485.0

445.0

15.0

490.0

440.0

20.0

240.0

1861-T009 HV

1861.39

540.0

435.0

40.0

546.0

429.0

46.0

1680.0

2104-T010 HV

2104.87

600.0

460.0

65.0

606.0

454.0

71.0

3640.0

Definition: T=Toroid shape; HP=High Precision; HV=High Voltage;CT= Current Transformer

*Customization: other dimensions are available to be customized.

 

Part Code

SWFNA-CT

Mean

Path

Length

mm

Outer

Diameter

a/mm

Inner

Diameter

b/mm

Height

c/mm

Outer

Diameter

(casing)

A/mm

Inner

Diameter

(casing)

B/mm

Height

(casing)

C/mm

Cross

Section

Ac/mm2

51-T001 ZS

51.84

14.3

9.9

10.0

17.3

8.0

13.0

17.6

54-T002 ZS

54.98

15.0

10.0

20.0

17.3

8.3

23.0

40.0

73-T003 ZS

73.83

20.0

13.0

18.0

24.0

11.5

21.0

50.4.

82-T004 ZS

82.47

23.0

16.5

20.0

27.0

15.2

23.0

52.0

85-T005 ZS

85.14

23.0

14.8

18.0

26.4

12.6

21.4

59.0

87-T006 ZS

87.18

23.0

13.5

15.0

26.0

11.5

18.0

57.0

89-T007 ZS

89.22

23.0

12.2

30.0

27.2

11.4

32.6

129.6

124-T008 ZS

124.09

32.0

17.0

12.0

35.0

15.0

15.0

72.0

Definition: T=Toroid shape; ZS=Zero-Sequence; CT= Current Transformer

*Customization: other dimensions are available to be customized.

 

Sunbow supplies a wide variety of magnetic cores made of amorphous ribbons and nanocrystalline ribbons.

 

Nanocrystalline Cores:

Cores for Current Transformers

Cores for Leakage Circuit Breakers

Cores for Switched Mode Power Supply

Nanocrystalline C-Cores

Nanocrystalline Circular Cut Cores

Nanocrystalline Common Mode Choke Cores

Precision Current Transformer Cores

 

Amorphous Cores:

Amorphous stator cores for Electric Motors

 

Cores for High Power Transformers

Cores for Medium Frequency Transformers

PFC Choke Cores

Rectangular Cut Cores

 

FAQ

 

Q: Are you trading company or manufacturer?

A: We are professional manufacturer specialized in the design,development and production of new-type amorphous,nanocrystalline,silicon steel sheets and other magnetic materials and components.

 

Q: What's your production capacity ?

A: The annual production capacity of amorphous&nanocrystalline ribbon is 600 tons;

The annual production capacity of power electronic core is 35 million;

C-type iron core annual production capacity of 240 tons;

The annual production capacity of reactors is 50,000;

The annual production capacity of precision transformers is 40 million;

 

Package:

 

product-1200-820

 

Three steps to start your customization today!

 

1. Tell us what you need,please call 021-63306968 Or send email to :sales@sunbowgroup.com

As every application has its own characteristics and requirements.
We provide customized services according to your application

Just tell us your design concept and basic parameters

 

2. Get solution & quote

We will work on the best solution and provide primarily specification& quote for your review.

 

3. Sample production and mass production

We will start mass production after customer confirmation and validation of samples.

 

our workshop

 

our workshop

 

our equipment

 

our equipment1

our equipment2

 

our testing

 

our testing1

our testing2

 

our certification

 

our certification

 

our production process

 

our production process

 

our exhibition

 

page-1200-1200

 

Hot Tags: nanocrystalline core for precision current transformer, China nanocrystalline core for precision current transformer manufacturers, suppliers, factory, Nano Core for Power Current Transformer, current transformer ferrite core, Nanocrystalline Core for Precision Current Transformer, nano toroidal core, an iron core in a transformer quizlet, nanocrystalline cores for leakage circuit breakers