New Fields And New Applications Of Amorphous And Nanocrystalline Soft Magnetic Alloys
Aug 21, 2026

· Develop amorphous alloy materials with high Bs (>1.8 T) and technologies for easy processing and forming.
· Achieve an energy-saving effect up to nearly 6 %, delivering remarkable energy-saving benefits.