Fe-Based Amorphous Alloy Strip
●Cores of distribution transformers (50-60Hz)
●Cores of medium frequency power transformers (400Hz-15KHz)
●Cores of switching power supply transformers (Below 15KHz)
Applications
●Cores of distribution transformers (50-60Hz)
●Cores of medium frequency power transformers (400Hz-15KHz)
●Cores of switching power supply transformers (Below 15KHz)
●Cores of filter reactors, filter and energy storage inductors, and power factor correction (PFC) inductors for (Below 50KHz)
●High-frequency rectangular cut cores of output inductors and transformers in switch mode power supply(SMPS), uninterruptible power supply (UPS) etc
●Cores of saturation reactors and pulse compressors
Performance Features
●Highest saturation magnetic induction among amorphous alloys --Minimize component size
●Low coercive force --Improve component efficiency
●Low iron loss (1/3 to 1/5 of silicon steel sheets) --Reduce component temperature rise Excellent temperature stabilit
Physical Properties
|
Saturation Magnetic Induction |
1.56T |
Curie Temp. |
410℃ |
|
Saturation Magnetostriction |
27*10-6 |
Crystallization Temp. |
550℃ |
|
Density |
7.18g/cm3 |
Hv Hardness |
960 |
|
Resistivity |
130μΩ·cm |
Conti. Operating Temp. |
-55-130℃ |
Magnetic Properties
|
Property |
Magnetic Field Annealing Transversal |
Annealing Without Magnetic Field |
Magnetic Field Annealing Longitudinal |
|
μm Max. Permeability |
>2*104 |
>20*104 |
>25*104 |
|
Saturation Magnetic Induction |
1.5T |
1.5T |
1.5T |
|
Residual Magnetic Induction |
<0.5T |
0.6-1.0T |
1.2T |
|
Coercive Force |
<4A/m |
<6A/m |
<2.5A/m |
|
(50Hz,1.4T) Loss (50Hz,1.4T) |
<0.2W/kg |
<0.13W/kg |
<0.25W/kg |
|
(400Hz,1.2T) Loss (400Hz,1.2T) |
<1.8W/kg |
<1.25W/kg |
<2W/kg |
|
(8KHz,1.2T) Loss (8KHz,1.2T) |
<80W/kg |
<60W/kg |
<100W/kg |
|
(-55-125℃) Iron Loss Variation (-55-125℃) |
<15% |
<15% |
<15% |
|
(120℃ 200 hour) Iron Loss Variation (120℃ 200 Hours) |
<15% |
<15% |
<15% |
Product Specification
|
Type |
(mm) Width |
(μm) Thickness |
Type |
(mm) Width |
(μm) Thickness |
|
1K101-5mm |
5±0.2 |
27±3 |
1K101-20mm |
20±0.2 |
27±3 |
|
1K101-8mm |
8±0.2 |
27±3 |
1K101-25mm |
25±0.2 |
27±3 |
|
1K101-10mm |
10±0.2 |
27±3 |
1K101-30mm |
30±0.2 |
27±3 |
|
1K101-15mm |
15±0.2 |
27±3 |
1K101-35mm |
35±0.2 |
27±3 |
Sunbow can produce other customized strips per user's request.
FAQ:
Q: Are you trading company or manufacturer?
A: We are professional manufacturer specialized in the design,development and production of new-type amorphous,nanocrystalline,silicon steel sheets and other magnetic materials and components.
Q: What's your production capacity ?
A: The annual production capacity of amorphous&nanocrystalline ribbon is 600 tons;
The annual production capacity of power electronic core is 35 million;
C-type iron core annual production capacity of 240 tons;
The annual production capacity of reactors is 50,000;
Package

our workshop

our equipment


our testing


our certification

our production process

our exhibition

Hot Tags: fe-based amorphous alloy strip, China fe-based amorphous alloy strip manufacturers, suppliers, factory, soft magnetic compoud, fe-based amorphous ribbon, fe based amorphous ribbon, amorphous ribbon 1K101, metglass, Soft Magnetic Materials
Send Inquiry