Iron-based Amorphous Alloy Ribbon
With a random atomic structure, the crystal anisotropy is not formed in amorphous alloy, so the alloy has an excellent soft magnetic property and the magnetic property of the alloy can be widely adjusted by a heat treatment process.
Product Introduction
With a random atomic structure, the crystal anisotropy is not formed in amorphous alloy, so the alloy has an excellent soft magnetic property and the magnetic property of the alloy can be widely adjusted by a heat treatment process.
Amorphous alloy is a new type of energy saving material produced by rapid solidification technology, being cooled from molten alloy at a rate of nearly million degrees per second. It has high permeability and low core loss because of the unique long-range disordered atomic structure, which is completely different from that of crystals. Amorphous alloy is widely used in the fields of distribution transformers, inductors, motor stators and sensors, taking the advantage of significantly improving device efficiency and reducing energy consumption.
Applications
● IF power transformer core
● Annular non-cut core for the switching power supply smoothing filter output inductor, differential mode input inductor
● Annular non-cut core for car audio noise suppression and car navigation system choking coil
● Annular cut core for PFC power factor correction in air conditioning and plasma TV
● High-frequency rectangular cutting core for output inductors and transformers of switching power supplies and uninterruptible power supplies
● Annular non-cut core of IGBTs, MOSFETs and GTOs pulse transformers
● Stator and rotor of high power density variable speed motor, and generator
Performance features
● Short strip production process and low production cost (see Fig. 1.1)
● The strip has excellent magnetic properties (Fig.1.2) and performance stability thanks to a special microstructure.
The composition and process parameters of the strip can be quickly adjusted to meet different application requirements.

Figure 1.1 Amorphous ribbon production process

Figure 1.2 Bs versus Hc of different soft magnetic materials
SWAR-Amorphous Roll Shear Strip

Table 1 Performance features of iron-based amorphous ribbons
|
Product code |
Ribbon width (mm) |
Ribbon thickness (μm) |
Saturation magnetic induction Bs (T) |
Coercivity Hc (A/m) |
Resistivity (μΩ·m) |
|
SWAR |
5~80 |
18~30 |
1.56 |
2.4 |
1.30 |
|
Saturation magnetostriction coefficient λs (ppm) |
Curie temperature Tc (℃) |
Crystallization temperature Tx (℃) |
Density ρ (g/cm3) |
Hardness Hv(kg/mm2) |
Thermal expansion coefficient (ppm/℃) |
|
27 |
410 |
535 |
7.18 |
960 |
7.6 |
FAQ:
Q: Are you trading company or manufacturer?
A: We are professional manufacturer specialized in the design,development and production of new-type amorphous,nanocrystalline,silicon steel sheets and other magnetic materials and components.
Q: What's your production capacity?
A: The annual production capacity of amorphous&nanocrystalline ribbon is 600 tons;
The annual production capacity of power electronic core is 35 million;
C-type iron core annual production capacity of 240 tons;
The annual production capacity of reactors is 50,000;
Q: What is your after-sales Guarantee?
A: For all problems encountered by customers, we will respond within 4 hours, and submit the solution within three working days.
Customer quotation response time is 24 hours.
It is planned to set up a "customer service center" in countries to flexibly respond to customer requirements and improve service levels.
The product warranty period is 30 months for product delivery or 24 months for product installation, and provides lifetime after-sales service.
The company is building a lean + agile supply chain, adding a customer order rapid processing process in the ERP system to ensure that the customer delivery time rate reaches 100%.
Perfect industrial chain and rich management experience over the years have enhanced Sunbow's competitive strength and anti-risk ability, making our products more competitive in price.
Package

Three steps to start your customization today!
1. Tell us what you need,you can call 021-63306968
Or send email to :sales@sunbowgroup.com
We supply nanocrystaline Soft Magnetic Material &Amorphous Soft Magnetic Material , please advise your request information:
1. Material Type
2. Application - Current Transformer, CMC, Audio, etc.?
3. Strips Width
4. Srips Thickness-- µm?
5. Potential Quantity -- kg?
2. Get solution & quote
We will work on the best solution and provide primarily specification& quote for your review.
3. Sample production and mass production
We will start mass production after customer confirmation and validation of samples.
our workshop

our equipment


our testing


our certification

our production process

our exhibition

Hot Tags: iron-based amorphous alloy ribbon, China iron-based amorphous alloy ribbon manufacturers, suppliers, factory, Fe based Amorphous Alloys, Amorphous Ribbons For Distribution Transformers, Magnetic Shields material, Finemet, amorphous 1k101, Iron based Amorphous Alloy Ribbon
Send Inquiry