Our nanocrystalline materials

Jan 24, 2025

1.Gravity ribbon 1K107

info-750-750

Main function and characteristics:

µi can reach 200k, µm can reach 700k, has advantages of high Bs (1.25T), high

permeability, low loss and so on.

Widely used in the production of precision current transformers, power current transformers, etc. Applied in power and electronics fields.

2.Pressure Ribbon 1K107B

info-750-750

Main function and characteristics:

Constant pressure ribbon making to achieve high

density, low thickness (12µm ~ 16µm), and good consistency. Widely used in high­frequency fields.

Widely used in high-frequency common mode inductors, high-power transformers, magnetic isolation sheets, etc.,

as well as inverter home appliances, new energy vehicles, wind and solar storage, wireless charging and other fields

3.Constant conductivity ribbon (SWFN035-200)

info-275-275

Main function and characteristics:

FN-series constant permeability nanocrystalline ribbon has high permeability linearity within 3500 20000,

has strong DC bias resistance, is widely used. Can substitute corresponding products of Hitachi, VAC and others.

Used in anti-DC precision metering transformers, high­power photovoltaic PCS converters, differential common­mode integrated inductors, AC and DC converter EMI filtering (vehicle, wind power, etc.), high-power pulse transformers and other fields