FERRITE GU CORES

FERRITE GU CORES

 

product-483-342
product-483-342

MODEL

G.W

SIZE(mm)

A

B

C

D

E

F

G

GU14/9

5

14.2±0.25

11.95±0.2

5.85±0.2

\

2.9±0.1

4.45±0.1

3.8±0.6

GU26/16

26

25.5±0.5

21.5±0.3

11.3±0.2

5.5±0.15

5.6±0.1

8.0±0.1

3.8±0.6

GU30/19

40

30.0±0.5

25.4±0.4

13.3±0.2

5.5±0.15

6.6±0.1

9.45±0.1

4.3±0.6

GU36/22

67

35.6±0.6

30.4±0.5

15.9±0.3

5.5±0.15

7.4±0.1

11.0±0.1

4.4±0.6

GU48/30

148

47.5±0.5

40.8min

19.2±0.4

5.8±0.2

10.6±0.3

14.8±0.3

8.4±0.6

GU50

178

50.0±0.5

44.0±0.5

16.0±0.3

\

17.0±0.3

20.0±0.3

6.2±0.6

 

MODEL

PARAMETER

AL±25%(nH/N^2)

N.W(g)

C1mm-1

Lemm

Aemm2

Vemm3

ZP40

GU14/9

0.790

19.8

25.1

495

2000

4.5

GU26/16

0.400

37.6

93.9

3530

4600

20.0

GU30/19

0.330

45.2

137.0

6190

5700

34.0

GU36/22

0.260

53.2

202.0

10700

7300

60.0

GU48/30

0.230

72.7

313.4

22780

7300

134.0

GU50

0.43

96.9

226.0

21900.0

5000

160