FERRITE UF Cores

FERRITE UF Cores

product-445-263

 

MODEL

G.WEIGHT

SIZE(mm)

A

Bmin

C

D

E

F

UF93

1580

93.0±2.5

36.5

28.0±0.5

28.0±0.5

49.5±1.0

79.0±1.0

UF96

1726

96.0±3.0

37.0

30.0±0.5

30.0±0.5

50.0±0.5

80.5±0.5

UF105

2810

105.0±3.0

39.0

30.0±0.5

40.0±1.0

65.0±1.0

95.0±1.0

UF120/80

2620

120.0±3.0

59.0

30.0±0.5

40.0±1.5

50.0±1.0

80.0±1.0

UF120/117

3550

120.0±3.0

59.0

30.0±0.5

40.0±1.5

87.0±1.0

117.0±1.0

 

MODEL

PARAMETER

AL±25%(nH/N^2)

N.WEIGHT (g)

C1mm-1

Lemm

Aemm2

Vemm 3

ZP40

ZH5K

ZH7K

ZH10K

UF93

0.45

362.0

797.0

289000.0

5000

 

 

 

1450

UF96

0.41

369.0

900.0

331695.0

5000

 

 

 

1490

UF105

0.39

471.0

1200.0

564000.0

6500

 

 

 

2700

UF120A

0.34

407.0

1184.6

482098.0

6100

 

 

 

2290

UF120B

0.47

564.0

1200.0

677000.0

4800

 

 

 

3020

 