Power Transformer Rectangular Core
High-frequency transformers for auxiliary power supplies of rail transit vehicles, insulated power converters, and inverter welders. High-frequency boosting transformers used in high-voltage power supplies for medical equipment and electrostatic precipitators.
Application
High-frequency transformers for auxiliary power supplies of rail transit vehicles, insulated power converters, and inverter welders. High-frequency boosting transformers used in high-voltage power supplies for medical equipment and electrostatic precipitators.
Performance features
The use of nanocrystalline soft magnetic material with low loss and high saturation flux density reduces the loss of high frequency transformer, and reduce the size and reduce the weight.
Figure 9.1 Loss versus frequency of different cores

Figure 9.2 DC B-H curve

Figure 9.3 Permeability versus frequency
Sunbow also produce the following nanocrystalline cores: nanocrystalline cut cores, nanocrystalline toroidal cores, nanocrystalline transformer core, nanocrystalline tape wound cores, nanocrystalline cores for current transformers, nanocrystalline cores for common mode cokes, nanocrystalline c core, nanocrystalline powder cores, nanocrystalline magnetic core, etc
Welcome to contact us to get more information.
Three steps to start your customization today!
1. Tell us what you need
As every application has its own characteristics and requirements.
We provide customized services according to your application
Just tell us your design concept and basic parameters
We design & produce goods based on clients' specifications & drawing:
1.Bare core size, Size finished
2.Al requirement @ different frequency
2. Get solution & quote
We will work on the best solution and provide primarily specification& quote for your review.
3. Sample production and mass production
We will start mass production after customer confirmation and validation of samples.
FAQ
Q: Are you trading company or manufacturer?
A: We are professional manufacturer specialized in the design,development and production of new-type amorphous,nanocrystalline,silicon steel sheets and other magnetic materials and components.
Q: What's your production capacity ?
A: The annual production capacity of amorphous&nanocrystalline ribbon is 600 tons;
The annual production capacity of power electronic core is 35 million;
C-type iron core annual production capacity of 240 tons;
The annual production capacity of reactors is 50,000;
Package:

our workshop

our equipment


our testing


our certification

our production process

our exhibition

Hot Tags: power transformer rectangular core, China power transformer rectangular core manufacturers, suppliers, factory, wound cores, nanocrystalline magnetic core, nanocrystalline cores for current transformer, Measurement Transducer Core, o core transformer, Coated Tape Wound Core