FERRITE TOROID CORES

FERRITE TOROID CORES

product-288-179

 

MODEL

G.W

SIZE

PARAMETER

AL±25%(nH/N^2)

N.W(g)

A

B

C

C1

Le

Ae

Ve

ZP40

ZH5K

ZH7K

ZH10K

H22/14/8

8.7

22.0±0.4

14.0±0.4

8.0±0.4

1.74

54.7

31.4

1720

1660

3980

5060

8110

10.5

H22/14/10

11

22.0±0.4

14.0±0.4

10.0±0.4

1.39

54.7

39.3

2150

2000

4950

6300

9000

10.5

H22/14/15

16.5

22.0±0.4

14.0±0.4

15.0±0.4

0.93

54.7

58.8

3215

3100

7400

9450

13500

16.0

H25/15/10

14.8

25.0±0.5

15.0±0.5

10.0±0.3

1.23

60.2

48.9

2944

2450

5100

7650

10200

14.0

H25/15/12

18

25.0±0.5

15.0±0.5

12.0±0.3

1.03

60.2

58.5

3520

2820

6740

8580

11500

17.5

H25/15/13

18

25.0±0.5

15.0±0.5

13.0±0.3

1.03

60.2

58.5

3520

2820

6740

8580

11500

 

H31/19/7

 

 

 

 

 

 

 

 

 

 

 

/

28.0

H31/19/13

29

31.0±0.6

19.0±0.4

13.0±0.4

0.99

75.5

76.3

5759

2900

6980

8850

/

28.0

H31/19/15

34

31.0±0.6

19.0±0.4

15.0±0.5

0.86

75.5

88.2

6660

3350

8000

10100

/

32.8

H36/23/15

 

 

 

 

 

 

 

 

 

 

 

/

53.0

H38/19/13

55

38.0±1.0

19.0±0.8

13.0±0.5

0.702

82.7

117.8

9750

4000

8900

 

/

53.0

H38/19/15

92

38.0±1.0

19.0±0.8

22.0±0.5

0.41

82.6

200.2

16535

7000

16000

21000

/

90.0

H45/26/12

60.5

45.0±1.5

26.0±1.2

12.0±0.6

0.92

103.8

112.5

11675

3030

7240

9200

/

58.5

H47/27/15

84

47.0±1.1

27.0±0.8

15.0±0.5

0.76

110

145

16050

3800

/

/

/

81.0

H49/31.8/15

79

49.0±1.2

31.8±0.9

15.0±0.4

0.97

123

126

15526

3000

/

/

/

74.5

H49/31.8/19

101

49.0±1.2

31.8±0.9

19.0±0.4

0.76

123

160

19730

3800

/

/

/

95.0

H50/25/20

140

50.0±1.2

25.0±0.5

20.0±0.4

0.456

108.6

237.9

25850

6300

 

 

 

135.0

H50/30/20

120

50.0±1.2

30.0±0.6

20.0±0.4

0.62

120.2

194

23400

4600

 

 

 

115.0

H56/28/28

250

56.0±1.2

28.0±0.8

28.0±0.6

0.324

122.7

377

46200

8800

/

/

/

240.0

H56/32/18

144

56.0±1.2

32.0±0.8

18.0±0.5

0.634

131.3

207

27200

4500

12000

/

/

139.0

H63/38/25

245

63.0±1.7

38.0±1.1

25.0±0.5

0.49

151.2

308.4

46622

5500

12600

17700

/

236.0

H70/44/32

360

70.0±1.5

44.0±1.0

32.0±0.5

0.428

173.5

404.1

70000

6700

 

 

/

347.0

H80/52/20

282

80.0±2.0

52.0±1.5

20.0±1.0

0.73

201.2

275

55324

3900

 

 

/

272.0

H85/55/20

335

85.0±2.0

55.0±1.5

20.0±1.0

0.72

212.9

294.2

62646

4000

 

 

/

323.0

H100/50/10

534

100.0±3.0

50.0±2.5

10.0±1.5

0.91

217.7

239.4

52117

3150

 

 

/

270.0

H100/50/20

309

100.0±3.0

50.0±2.5

20.0±1.5

0.45

216.9

477.9

103699

6400

 

 

/

550.0

H100/60/15

393

100.0±2.5

60.0±2.0

15.0±0.5

0.825

240

291.2

70200

3400

 

 

/

360.0

H102/65/20

495

102.0±3.0

65.0±3.0

20.0±1.5

0.7

253.1

362.1

91630

4100

 

 

/

465.0

H118/80/22

1060

118.0±3.0

80.0±3.0

35.0±1.5

0.46

303.6

653.9

198541

6250

 

 

/

982.0

H124/60/20

925

124.0±3.5

60.0±3.0

20.0±1.5

0.88

265.4

301.5

80004

3250

 

 

/

860.0

H124/60/40

1710

124.0±3.5

60.0±3.0

40.0±2.0

0.22

262.3

1207.2

316646

13000

 

 

/

1600.0

Hot Tags: ferrite toroid cores, China ferrite toroid cores manufacturers, suppliers, factory, ferrite core transformer, EMI ferrite EMI ferrites, ferrite ring ferrite rings, UU core, PLC ferrite core PLC ferrite cores, ferrite core