FE-SI CORE

FE-SI CORE

MODEL :GS250060
Other company referance model NO.:TMS610060,FM610060

Shape and Dimensions

 

product-448-124

  1. Shape and Dimensions
  2. Appearance Requirement
  3. Electromagnetic and Mechanical properties
  4. Material Characteristics
  5. Package
  6. Inspection Rules
  7. Note
  8. Version information

 

Appearance Requirement

 

The surface should be smooth, without blistering, and blotch after coating, and no serious chips.

 

Electromagnetic and Mechanical properties

 

(Item)

(Standard)

(Test conditions)

L0 Inductance

(172.8±13.82)μH

TH2816B,100KHz,1.0V,0.8mm*30Ts

Q Value

≥40

TH2816B,100KHz,1.0V,0.8mm*30Ts

L38A Inductance

≥117.5μH

TH2829C+TH1778,100KHz,1.0V, 0.8mm*30Ts,IDC=38A

Core loss

≤190mw/cm3

WL3866+CH2335A 50KHz/50mT

(Hi-POT)

>1500 Vac

CC2670A 50Hz,0.5mA, 3Sec.

Material

F060

 

Coating Material

Epoxy Resin

Coating Color

Blue

 

Material Characteristics

 

product-721-376

product-745-392

 

 

Typical values of materials are listed in the figure for designers' reference.

 

Package

 

The product is packed with cardboard pallet, 13*4, 52 pieces in total. The outer box is labeled with identification card as required.

 

Inspection Rules

 

Product acceptance according to provisions of GB/T2828.1-2003, with its examination level: appearance, size II, L, Q value S3, AQL 0.65.

Customers should be complete acceptance check in one month and notify us the results in write; otherwise we take the products as acceptance.

 

Hot Tags: fe-si core, China fe-si core manufacturers, suppliers, factory, Zinc ferrite, core powder, FE SI alloy, iron powder toroid core, powder core, special shape magnetic powder cores