Application Of Amorphous And Nanocrystalline Soft Magnetic Alloy Materials (High Frequency Transformer)
Sep 01, 2025
- High saturate induction-reduce volume of transformers
- High permeability and low coercivity- improve efficiency, lower exciting power and reduce copper loss
- Low core loss-reduce temperature rise of transformers
- Excellent thermal stability-with the serving temperature of -55℃~130℃ for long time