Manufacturing Process Of Amorphous & Nanocrystalline Soft Magnetic Alloy Materials
Jan 12, 2026
Amorphous Preparation Method - Planar Flow Casting (PFC) Ribbon Process
- Cooling Rate: 106 ℃/s
- Roll Speed: 30 m/s
- Ribbon Thickness: 0.01 – 0.03mm
Jan 12, 2026
Amorphous Preparation Method - Planar Flow Casting (PFC) Ribbon Process