Fe-Based Nanocrystalline Alloy Strip
Nanocrystalline alloy is composed of ferrum, silicon, boron and a small amount of copper, molybdenum, niobium, nickel and cobalt; amongst which copper and niobium are essential elements to obtain the nanocrystalline structure.
Features:
Nanocrystalline alloy is composed of ferrum, silicon, boron and a small amount of copper, molybdenum, niobium, nickel and cobalt; amongst which copper and niobium are essential elements to obtain the nanocrystalline structure. After annealing treatment with appropriate temperature, the nanocrystalline alloy strip forms crystalline grains with the size of 10-20nm and a dispersed structure. The structure has very excellent magnetic properties, including high Saturation magnetic induction; high magnetic permeability; low coercive force; low loss; good temperature stability, wear resistance, corrosion resistance; as well as lower price with the best performance/price of all metal soft magnetic materials. Nanocrystalline alloy material is cheap, but the magnetic properties can be excellent, almost comparable to the cobalt-based amorphous alloy. It is ideal material for industrial and civil high-frequency transformers, mutual inductors, inductors, and for replacement of permalloy and ferrite products. With the above mentioned magnetic performance characteristics, the Fe-based nanocrystalline alloy has the following advantages in magnetic applications:
1. High Saturation magnetic induction Bs - being capable of reducing the size of transformers
2. High magnetic permeability and low coercive force - being capable of improving the efficiency of transformers and the sensitivity of mutual inductors, reducing the coil distribution parameters, reducing the number of turns of common mode inductors, reducing copper loss
3. Low loss - being capable of reducing the temperature rise of transformers
4. Good stability - being capable of long-term work under working condition of high temperature (130 ℃)
5. Lower price - the best performance/cost of all metal soft magnetic materials.
Physical Properties:
|
Saturation Magnetostriction |
<2*10-6 |
Saturation Magnetic Induction |
1.25 T |
|
Density, d |
7.2g/cm3 |
Curie Temp. |
560℃ |
|
Resistivity |
130μΩ·cm |
Crystallization Temp. |
510℃ |
|
Conti. Operating Temp. |
-55-130℃ |
Hardness |
880Hv |
Magnetic Properties:
|
Property |
Annealing Without Magnetic Field |
Magnetic Field Annealing Transversal |
Magnetic Field Annealing Longitudinal |
|
Initial permeability |
>8*104 |
>2*104 |
>1*104 |
|
Max. permeability |
>45*104 |
>5*104 |
>50*104 |
|
Residual Magnetic Induction |
0.6T |
<0.2T |
>0.85T |
|
coercive force |
<0.8A/m |
<1.8A/m |
<1.8A/m |
|
Iron Loss P (20Hz,0.5T) |
<25W/kg |
<50W/kg |
<90W/kg |
|
Iron Loss P (100KHz,0.3T) |
<150W/kg |
<150W/kg |
<300W/kg |
|
Iron Loss Variation(-55-125℃) |
<15% |
<15% |
<15% |
Product Specification
|
Type |
Width(mm) |
Thickness(μm) |
Type |
Width(mm) |
Thickness(μm) |
|
1K107-5mm |
5±0.2 |
30±5 |
1K107-20mm |
20±0.2 |
30±5 |
|
1K107-6.5mm |
6.5±0.2 |
30±5 |
1K107-25mm |
25±0.2 |
30±5 |
|
1K107-8mm |
8±0.2 |
30±5 |
1K107-30mm |
30±0.2 |
30±5 |
|
1K107-10mm |
10±0.2 |
30±5 |
1K107-35mm |
35±0.2 |
30±5 |
|
1K107-15mm |
15±0.2 |
30±5 |
|
|
|
※SUNBOW can produce other customized strips per user's request.
Three steps to start your customization today!
Tell us what you need
We supply nanocrystaline Soft Magnetic Material &Amorphous Soft Magnetic Material , please advise your request information:
1.Material Type
2.Application - Current Transformer, CMC, Audio, etc.?
3.Strips Width
4.Srips Thickness-- µm?
5.Potential Quantity -- kg?
Get solution & quote
We will work on the best solution and provide primarily specification& quote for your review.
Sample production and mass production
We will start mass production after customer confirmation and validation of samples.
Package:

our workshop

our equipment


our testing


our certification

our production process

our exhibition

Hot Tags: fe-based nanocrystalline alloy strip, China fe-based nanocrystalline alloy strip manufacturers, suppliers, factory, nanocrystalline strip, nanocrystalline steel, nano ribbon 1K107B, Nanocrystalline Straight Spray Strip, nano ribbon, 1k107B
Send Inquiry