Iron-based Nanocrystalline Ribbons
An amorphous ribbon is formed by rapidly quenching molten metal composed of iron, silicon, boron and a small amount of copper and niobium at 106 ° C / s. The amorphous ribbon is heat treated above the crystallization temperature to obtain nanocrystals (~10 nm) having a very small size and uniform distribution, and the microstructure has better soft magnetic properties than the amorphous alloy.
Product Introduction
An amorphous ribbon is formed by rapidly quenching molten metal composed of iron, silicon, boron and a small amount of copper and niobium at 106 ° C / s. The amorphous ribbon is heat treated above the crystallization temperature to obtain nanocrystals (~10 nm) having a very small size and uniform distribution, and the microstructure has better soft magnetic properties than the amorphous alloy.
Sunbow produces various types of soft magnetic materials, including iron-based amorphous alloys and iron-based nanoalloys, and these materials are used in our products. We continually make technical improvements and develop new applications with the unique properties of these materials. Iron-based nanocrystalline materials are superior to traditional materials and will be the best solution for your application (Figure 2.1).

Figure 2.1 μr versus Bs of different soft magnetic materials
Application
●Iron cores used in the switching power supply transformer and pulse transformer
●Iron cores used in power transformer and precision current transformer
●Iron core used in the leakage protection switch transformer
●Iron core used in filter inductor, energy storage inductor, and reactor
●EMC common mode and differential mode inductor core
●Saturation reactor, magnetic amplifier, peak suppressor core and magnetic beads
Performance features
High saturation magnetic induction (1.25 T) and high magnetic permeability (>80,000) for small size and high precision
●Iron loss is equivalent to 1/5 of iron-based amorphous, and loss at ,100 kHZ, 300 mT is as low as 70 W/kg
●Saturation magnetostriction coefficient close to 0, with very low operating noise
●With excellent temperature stability, material performance change rate <10% in the temperature range of -50~120 °C
●With the excellent frequency characteristics, excellent magnetic permeability and low loss over a wide frequency range
●With adjustable magnetic properties, different types of magnetic properties can be obtained by applying different transverse and vertical magnetic fields, or without magnetic field heat treatment, such as low remanence, high rectangular ratio, and high magnetic permeability
Three steps to start your customization today!
Tell us what you need
We supply nanocrystaline Soft Magnetic Material &Amorphous Soft Magnetic Material , please advise your request information:
1.Material Type
2.Application - Current Transformer, CMC, Audio, etc.?
3.Strips Width
4.Srips Thickness-- µm?
5.Potential Quantity -- kg?
Get solution & quote
We will work on the best solution and provide primarily specification& quote for your review.
Sample production and mass production
We will start mass production after customer confirmation and validation of samples.
Package:

our workshop

our equipment


our testing


our certification

our production process

our exhibition

Hot Tags: iron-based nanocrystalline ribbons, China iron-based nanocrystalline ribbons manufacturers, suppliers, factory, nanocrystalline magnet ribbons, nanocrystalline magnetic ribbons, Nanocrystalline products, Iron based Nanocrystalline Ribbons, nano strip, nano ribbon 1K107B
Send Inquiry