Product Introduction

Table 2.1 Performance features of iron-based nanocrystalline materials
|
Product code |
Ribbon width (mm) |
Ribbon thickness (μm) |
Saturation magnetic induction Bs(T) |
Coercivity Hc (A/m) |
Resistivity (μΩ·m) |
|
SW03 |
5~60 |
26~32 |
1.25 |
1.5 |
1.20 |
|
Saturation magnetostriction coefficient λs (ppm) |
Curie temperature Tc (℃) |
Crystallization temperature Tx (℃) |
Density ρ(g/cm3) |
Hardness Hv (kg/mm2) |
Thermal expansion coefficient (ppm/℃) |
|
1 |
570 |
- |
7.2 |
- |
- |
Three steps to start your customization today!
Tell us what you need
We supply nanocrystaline Soft Magnetic Material &Amorphous Soft Magnetic Material , please advise your request information:
1.Material Type
2.Application - Current Transformer, CMC, Audio, etc.?
3.Strips Width
4.Srips Thickness-- µm?
5.Potential Quantity -- kg?
Get solution & quote
We will work on the best solution and provide primarily specification& quote for your review.
Sample production and mass production
We will start mass production after customer confirmation and validation of samples.
Package:

our workshop

our equipment


our testing


our certification

our production process

our exhibition

Hot Tags: nanocrystalline straight spray strip, China nanocrystalline straight spray strip manufacturers, suppliers, factory, 1k107B, Nanocrystalline Ribbon 1K107, nanocrystalline magnetic materials, 1K107, nanocrystalline magnetic ribbons, nanocrystalline alloy ribbon
Send Inquiry