NANO-CRYSTALLINE COMMON MODE CHOKE CORE
NANO-CRYSTALLINE COMMON MODE CHOKE CORE
video
NANO-CRYSTALLINE COMMON MODE CHOKE CORE
choke
ef286246e7540f62bf6c9d9adfecf52
EMC。
1/2
<< /span>
>

NANO-CRYSTALLINE COMMON MODE CHOKE CORE

Nanocrystaline ribbon is the soft magnetic alloy material with superfine grain size(~10nm) which is formed by the Fe、Si、 B、Cu、Nb and other elements,and gets through specfic annealing process at cooling rate of 10 ℃/s.6

Nanocrystaline ribbon is the soft magnetic alloy material with superfine grain size(~10nm) which is formed by the Fe,Si, B,Cu,Nb and other elements,and gets through specfic annealing process at cooling rate of 10 ℃/s.6

The outstanding feature of this new metalic material is short manufacturing process, forming by one-step and saving energy consumption.It has the feature of high saturation magnetization (Bs) of Fe- based crystalline alloy and high permeablty and low loss of Co-based crystalline alloy,so it can satisty the performance requirements of high frequency and low loss. This material is mainly applied in the production of high-end common mode chokes, high frequency transformer, all kinds of current transformers and high-end magnetic ampliier, etc. Related cores and components are mainly used in new energy vehicle power management system, drive system, wireless charging module for mobile phone, rail transit, the precipitation power, grid- connected photovoltaic inverter, digital electronic products, and smart meters in the power grid to meet the requirement of high frequency, large current, miniaturization and energy-saving.

NANO-CRYSTALLINE COMMON MODE CHOKE CORE

 

Application

 

Inverter circuit

Frequency converter

UPS

Switching Mode Power

EMC filter

 

product-397-396

 

Characteristic

 

High saturate induction - reduce volume of CMC

Excellent impedance frequency characteristic

Outstanding ability to resist unbalanced current

product-820-430

Excellent temperature stability

 

SQ COMMON MODE SERIES CORE

Characteristic

Better EMI suppression effect

Flat wire vertical winding scheme can be adopted, with extremely low distributed capacitance and better heat dissipation effect

Avoiding performance degradation caused by stress on the core

 

Working principle of common mode inductor

 

When the normal current flows through the common mode inductor in the circuit, the current will produce reverse magnetic field in the same phase winding inductor coil to cancel each other. At this time, the inductance is approximately zero and the impedance to the input current is very small.

 

When the coil passes through the coil, the common mode current wil be attenuated, and the coil will produce a common mode current.

 

Therefore, the larger the impedance of the common mode inductor, the better the common mode filtering effect. In a certain frequency range, nanocrystalline materials have higher impedance than traditional materials ferrite. Compared with ferrite, the initial permeability of nanocrystals is much higher, so the volume can be smaller, the winding coils are less, the distributed capacitance is smaller, and the impedance characteristics are better.

 

Sunbow Part No.

Core dimensions

Finished core dimensions

Effictive cross section

Mean path length

Permeability(at 10KHZ)

AL Nominal Value**

 

OD×ID×HT

OD×ID×HT

AFe

lFe

Interval value

Refere nce

value

10kHz

100kHz

 

mm

mm

cm2

cm

   

μH

μH

SW-CM120805

Φ12×8×5

Φ14.3×6.8×6.9

0.08

3.1

50000-120000

90000

28

6.7

SW-CM151005

Φ15×10×5

Φ17.1×8.3×7.1

0.09

3.9

50000-120000

91000

29

6.8

SW-CM201208

Φ20×12.5×8

Φ22.6×10.3×10.2

0.24

5.1

50000-120000

97000

56

14

SW-CM201210

Φ20×12×10

Φ22.6×10.5×12.5

0.31

5

50000-120000

85000

62

15

SW-CM211510

Φ21×15×10

Φ23.5×13.1×12.3

0.23

5.7

50000-120000

85000

43.5

9.2

SW-CM252065

Φ25×20×6.5

Φ26.8×18.7×7.9

0.12

7.1

50000-120000

80000

17.1

3.8

SW-CM252010

Φ25×20×10

Φ28×17.2×13.2

0.2

7.1

50000-120000

80000

28

7.2

SW-CM251610

Φ25×16×10

Φ28×14×13.1

0.35

6.4

50000-120000

90000

67

15

SW-CM261610

Φ26×16×10

Φ28.3×14×12.8

0.39

6.6

50000-120000

90000

57

14

SW-CM302010

Φ30×20×10

Φ33.2×17.8×13.3

0.39

7.9

50000-120000

90000

60

14

SW-CM302015

Φ30×20×15

Φ33.6×17.8×17.2

0.59

7.9

50000-120000

96000

88

20

SW-CM322010

Φ32×20×10

Φ34.4×18.1×13

0.47

8.2

50000-120000

95000

57

14

SW-CM402515

Φ40×25×15

Φ44.5×21.8×18.8

0.88

10.2

50000-120000

94000

99

23

SW-CM403215

Φ40×32×15

Φ44.5×29×19

0.47

11.3

50000-120000

90000

48

11

SW-CM453015

Φ45×30×15

Φ48.3×26.4×18.2

0.88

11.8

50000-120000

95000

87

20

SW-CM503215

Φ50×32×15

Φ53.8×28.5×18.2

1.4

12.9

50000-120000

90000

100

27

SW-CM504020

Φ50×40×20

Φ53.6×37×23.2

0.78

14.1

50000-120000

80000

45

14

SW-CM635025

Φ63×50×25

Φ69×46×29

1.27

17.7

50000-120000

90000

59

18

SW-CM644020

Φ64×40×20

Φ68.2×37×23.5

1.87

16.3

50000-120000

90000

115

29

SW-CM805020

Φ80×50×20

Φ83.8×46.6×24.8

2.34

20.4

50000-120000

95000

94

28

SW-CM906020

Φ90×60×20

Φ95.4×55×24.5

2.34

23.6

50000-120000

90000

90

25

SW-CM1027625

Φ102×76×25

Φ107×70.3×29.7

2.54

27.9

50000-120000

95000

91

22

 

Note: The above table only lists some products. The specification and performance of nanocrystalline core can be customized according to customer's requirements. Please contact us for details.

Hot Tags: nano-crystalline common mode choke core, China nano-crystalline common mode choke core manufacturers, suppliers, factory, o type transformer, nanocrystalline iron core, Pulse Power Cores, magnetic cores for current transformers, nanocrystalline CMC core, power transformer toroidal core