What are the types of soft magnetic materials
Oct 12, 2023
① Pure iron and low-carbon steel
Carbon content below 0.04%, including electromagnetic pure iron and electrolytic iron. Its characteristics are high saturation magnetization, low price, and good processing performance; But its low resistivity and high eddy current loss under alternating magnetic fields are only suitable for static use, such as manufacturing electromagnetic iron cores, pole shoes, relay and speaker magnetic conductors, magnetic shielding covers, etc.
② Ferrosilicon alloy
The silicon content ranges from 0.5% to 4.8%, commonly known as silicon steel sheet, and is generally used as a thin plate. Adding silicon to pure iron can eliminate the phenomenon of magnetic materials changing with usage time. As the silicon content increases, the thermal conductivity decreases, the brittleness increases, and the saturation magnetization strength decreases. However, its resistivity and magnetic permeability are high, and its coercive force and eddy current loss are reduced. Therefore, it can be applied to the field of AC, manufacturing iron cores for motors, transformers, relays, transformers, etc.
③ Iron aluminum alloy
Containing 6% to 16% aluminum, it has good soft magnetic properties, high permeability and resistivity, high hardness, good wear resistance, but brittleness. It is mainly used for manufacturing iron cores and magnetic heads for small transformers, magnetic amplifiers, relays, and ultrasonic transducers.
④ Iron silicon aluminum alloy
Obtained by adding silicon to a binary iron aluminum alloy. Its hardness, saturation magnetic induction intensity, magnetic permeability, and resistivity are all high. The disadvantage is that magnetic properties are sensitive to component fluctuations, have high brittleness, and have poor processing performance. Mainly used for audio and video heads.
⑤ Nickel iron alloy
Nickel content ranges from 30% to 90%, also known as permalloy. Through alloying element ratios and appropriate processes, magnetic properties can be controlled to obtain soft magnetic materials such as high magnetic conductivity, constant magnetic conductivity, and moment magnetic properties. It has high plasticity and is sensitive to stress, and can be used as a material for pulse transformers, inductor cores, and functional magnetic materials.
⑥ Iron cobalt alloy
The cobalt content ranges from 27% to 50%. Has high saturation magnetization and low resistivity. Suitable for manufacturing pole shoes, motor rotors and stators, small transformer cores, etc.
⑦ Soft magnetic ferrite
Non metallic ferrous magnetic soft magnetic materials. High resistivity (10-2-1010 Ω · m), lower saturation magnetization than metals, and low price, widely used as inductance and transformer components (see ferrite).
⑧ Amorphous soft magnetic alloy
A non long-range ordered, grain free alloy, also known as metallic glass or amorphous metal. It has high magnetic permeability and resistivity, low coercivity, insensitivity to stress, and no magnetic crystal anisotropy caused by crystal structure. It has characteristics such as corrosion resistance and high strength. In addition, its Curie point is much lower than that of crystalline soft magnetic materials, greatly reducing electrical energy loss, and making it a new type of soft magnetic material being developed and utilized.
⑨ Ultra microcrystalline soft magnetic alloy
A soft magnetic material discovered in the 1980s. Composed of crystalline and amorphous grain boundary phases less than 50 nanometers, it has better comprehensive properties than crystalline and amorphous alloys. It not only has high magnetic permeability, low coercive force, low iron loss, but also high saturation magnetic induction strength and good stability. The main research focus is on iron based ultra microcrystalline alloys.