FERRITE EC CORES

FERRITE EC CORES

product-326-285

 

MODEL

G.W

SIZE(mm)

A

B min

C

D

E

F

EER26/19

12.4

25.5±0.6

19.8

7.5±0.3

7.5±0.3

6.6±0.3

9.5±0.3

EC28/20

25

28.5±0.5

21.8

9.9±0.3

11.4±0.3

6.0±0.2

10.0±0.2

EC28/28

33

28.5±0.5

21.8

9.9±0.3

11.4±0.3

10.0±0.2

14.0±0.2

EC28/34

36

28.5±0.5

21.8

9.9±0.3

11.4±0.3

13.0±0.2

17.0±0.2

EER29/16

31.2

29.8±0.5

22

9.5±0.3

9.5±0.3

11.4±0.2

16.0±0.2

EC29/28

33.6

29.4±0.6

22.3

9.9±0.3

11.4±0.3

10.0±0.2

14.0±0.2

EC29/34

37

29.4±0.5

22.3

9.9±0.3

11.4±0.3

13.0±0.2

17.0±0.2

EC32/24

48

31.8±0.5

26.6

13.2±0.2

20.2±0.3

9.2±0.2

12.0±0.2

ETD29/16

31.2

29.8±0.8

22

9.5±0.3

9.5±0.3

11.0±0.2

15.8±0.2

EC34/32

36.5

34.0±0.5

22

15.6±0.2

15.6±0.3

10.6±0.2

16.0±0.2

ETD34/35

44.4

34.2±0.8

25.6

10.8±0.3

10.8±0.3

12.3±0.3

17.5±0.3

ETD35/35

45

35.2±0.8

26.4

10.8±0.3

10.8±0.3

12.3±0.3

17.5±0.3

EC35/30

43.6

35.0±0.7

25.6

11.3±0.4

11.3±0.4

10.0±0.3

15.0±0.3

EC35/31

44

35.0±0.7

25.6

11.3±0.4

11.3±0.4

10.0±0.3

15.5±0.3

EC35/42

54

35.0±0.7

25.6

11.3±0.4

11.3±0.4

15.0±0.3

21.0±0.3

EC35/43

55

35.0±0.7

25.6

11.3±0.4

11.3±0.4

15.5±0.3

21.5±0.3

EC36/43

56.4

36.0±0.7

26.2

11.3±0.4

11.3±0.4

15.5±0.3

21.5±0.3

EC39/40

63

39.1±0.9

29.1

12.5±0.3

12.5±0.3

14.5±0.3

20.0±0.3

EC39/42

65

39.1±0.9

29.1

12.5±0.3

12.5±0.3

15.5±0.3

21.0±0.3

EC40/45

82

40.0±0.8

28.8

13.3±0.3

13.3±0.3

15.5±0.3

22.5±0.3

EER40/19/20

90

40.0±1.0

35.8

18.8±0.3

32.6±0.4

6.4±0.25

10.0±0.25

EC41/45

83

41.0±0.8

29.8

13.1±0.3

13.1±0.3

15.5±0.3

22.5±0.3

EC42/41/14.8

88

42.0±1.0

31.5

14.7±0.3

14.8±0.3

15.0±0.3

20.5±0.3

EC42/43/14.8

92

42.0±1.0

31.5

14.7±0.3

14.8±0.3

16.0±0.3

21.5±0.3

EC42/43/15.2

97.6

42.0±1.0

31.5

15.2±0.3

15.3±0.3

15.5±0.3

21.5±0.3

EC42/43/17.3

123

42.0±0.5

31.8

17.3±0.3

19.6±0.4

15.6±0.3

21.5±0.3

EC43/45/14.8

98

43.0±1.0

32.5

14.8±0.3

14.8±0.3

16.5±0.3

22.5±0.3

EC43/47

110

43.3±1.0

31.5

15.2±0.3

15.3±0.3

16.5±0.3

23.5±0.3

EC44/47

109

44.0±1.0

32.5

15.2±0.3

15.3±0.3

16.5±0.3

23.5±0.3

EC46/47

112

46.0±1.0

34

15.2±0.3

15.3±0.3

16.7±0.3

23.5±0.3

EC46/51

118

46.0±1.0

34

15.2±0.3

15.3±0.3

18.2±0.3

25.4±0.3

EC49/50

133

48.7±1.1

36.1

16.3±0.4

16.4±0.5

18.1±0.3

24.7±0.3

EC49.2/50

132

49.2±1.1

37.5

16.1±0.4

16.4±0.5

18.3±0.3

24.7±0.3

EC59/62

292

59.8±1.3

43.6

21.6±0.5

21.6±0.5

22.5±0.4

31.0±0.2

 

Model

PARAMETER

AL±25%(nH/N^2)

N.W(g)

C1mm-1

Lemm

Aemm2

Vemm3

ZP40

EC26/19

1.14

48.9

43.0

2103

1900

10.5

EC28/20

0.57

48.2

84.5

4079

3800

27.2

EC28/28

0.76

64.2

83.8

5376

2850

29.0

EC28/34

0.91

76.1

83.4

6353

2400

31.2

EER29/16

0.94

72.0

76.0

5742

2200

28.5

EC29/28

0.78

65.4

83.7

5474

2800

29.3

EC29/34

0.92

77.3

83.6

6462

2400

31.5

EC32/24

0.45

59.8

132.8

7946

4800

42.2

ETD29

0.96

70.6

73.6

7640

2500

28.0

EC34/32

0.35

67.5

132.8

7946

6180

64.3

ETD34/35

0.82

79.0

97.0

7660

2750

41.0

ETD35/35

0.82

80.1

97.0

7780

2700

40.0

EC35/30

0.65

70.1

108.4

7595

3300

38.0

EC35/31

0.65

70.1

108.4

7595

3300

38.5

EC35/42

0.81

90.9

112.0

10100

2600

48.0

EC35/43

0.90

92.2

112.0

10320

2550

50.0

EC36/43

0.85

93.5

112.0

10470

2500

51.0

EC39/40

0.70

91.9

130.7

12012

3100

56.2

EC39/42

0.73

95.9

130.6

12529

3000

59.0

EC40/45

0.66

98.0

149.0

14600

3250

73.0

EER40/19/20

0.20

52.6

268.5

14150

11000

80.0

EC41/45

0.67

99.0

147.5

14620

3200

73.6

EC42/41/14.8

0.58

96.0

163.0

15660

3700

82.0

EC42/43/14.8

0.58

99.7

168.0

16617

3700

85.0

EC42/43/15.2

0.53

98.5

184.0

18142

4000

90.0

EC42/43/17.3

0.42

98.5

233.0

23000

5100

108.0

EC43/45

0.59

103.1

173.4

17883

3650

85.5

EC43/47

0.55

104.0

191.0

20044

4000

100.0

EC44/47

0.55

104.0

191.0

20044

4000

100.0

EC46/47

0.57

107.5

187.5

20150

4000

102.0

EC46/51

0.55

104.0

191.0

20044

4000

100.0

EC49/50

0.53

114.0

213.0

24200

4100

120.0

EC49.2/50

0.58

118.0

206.0

24490

3700

117.0

EC59/62

0.38

139.0

368.0

51500

5400

257.0

Hot Tags: ferrite ec cores, China ferrite ec cores manufacturers, suppliers, factory, EMI ferrite EMI ferrites, ferrite EE cores, Mn Zn Ferrite cores, ferrite SQ core, Mn Zn power ferrite materials, Cylindrical Core Ferrites cylindrical cores ferrite

Send Inquiry

(0/10)

clearall