Nanocrystalline Cut Core
|
SPECIFICATION |
|||||||||
|
DESCRIPTION |
NANOCRYSTALLINE C CORE |
MATERIAL |
1K107B (Or equivalent) |
||||||
|
SUNBOW NO. |
DC-NTC-33/24*8 |
COATING COLOUR |
GREEN |
23.7/32.7*8.5 |
|||||
|
1:Appearance
|
CORE SIZE(mm) |
FINISHED (mm) |
|||||||
|
OD(A) |
32.5±0.3 |
33.5 MAX |
|||||||
|
ID(B) |
24.2±0.3 |
23.2 MIN |
|||||||
|
H(C) |
8.3±0.2 |
9.0 MAX |
|||||||
|
CUTTING THICKNESS |
0.8±0.1mm |
||||||||
|
Se |
0.25cm2 |
Lc |
8.98cm |
Duty factor |
0.80 |
||||
|
2:Test circuit diagram
|
|||||||||
|
3:Electrical characterization |
|||||||||
|
1 |
Test condition:N1:N2=1:1,100mA≥0.20 mV(1KHz,0.3V,30Ω,AL≥7.0uH) |
||||||||
|
4:Process description |
|
||||||||
|
No |
|
|
|||||||
|
1 |
Appearance |
The incision is smooth , without stains; Two pairs of semi-symmetric drop ≤1.0mm |
|||||||
|
2 |
Package |
Cardboard in rows of blister packaging |
|||||||
Hot Tags: nanocrystalline cut core, China nanocrystalline cut core manufacturers, suppliers, factory, precision current transformer cores, precision current transformer core, magnetic cores for current transformers, PFC Choke Cores, Coated Tape Wound Core, nanocrystalline ring nanocrystalline rings