Amorphous And Nanocrystalline Cores Application
Jun 03, 2024
Applications
Can Replace similar types of silicon steel power transformers
Features
- High saturation magnetic induction intensity---- reduction in core volume;
- Rectangular structure - easy to assemble coil;
- Core opening - excellent resistance to DC bias saturation;
- Low loss - reduce temperature rise (1/5-1/10 of silicon steel);
- Good stability - can work for a long time at -55-155 ℃.