Magnetic Shielding Sheets
Amorphous & Nanocrystalline magnetic shielding sheets adopt high Bs amorphous & nanocrystalline ribbons developed by our company independently as the soft magnetic material.
Product Introduction
Amorphous & Nanocrystalline magnetic shielding sheets adopt high Bs amorphous & nanocrystalline ribbons developed by our company independently as the soft magnetic material. Compared with ferrite magnetic shielding sheet, they have the performance advantages of higher peremeability and higher design power, with thin thickness, excellent flexibility, easy processing and wide working frequency range, which apply to the magnetic shielding of various electronic products. For wireless charging application, the shielding sheet performs well in high power wireless charging with its arbitrarily adjustable permeability and excellent anti-saturation current.
They effectively improve the power and speed of wireless charging and significantly reduce the weight, volume and temperature rise of wireless charging modules, which are the best choice for
high-power and fast wireless charging. magnetic shielding sheets made of single-layer or multi-layer high-quality amorphous or nanocrystalline ribbon offer high permeability and low core losses. It can effectively reduce the EMI of magnetic field to the surroundings. It is widely used in aerospace, automotive, communications and other electronic equipment as EMI resistance, electromagnetic screen and wireless charging. magnetic shielding sheets are classified as amorphous shielding sheets and nanocrystalline shielding sheets according to different kinds of soft magnetic materials.
Application Field
Wireless charging and electromagnetic shielding of various electronic products
NFC modules
Product Size
Product structure diagram:

Figure 1 Magnetic Shielding Roll Material

Figure 2 Magnetic Shielding Sheets
|
Coiled material model |
Case |
width |
Number of Layers |
Permeability |
|
SWNR |
Figure 1 |
20-200 |
1-20 |
600-8000 |
|
SWNS |
Figure 2 |
All can be customized |
1-20 |
600-8000 |
Figure 2 Magnetic Shielding Sheets
Note: 1. Specifications can be customized according to customers' requirements.
2.If the number of nanocrystalline layers is more than six layers, it shall be packaged according to the maximum length of two meters.
For additional information and immediate assistance with your requirements, designs and applications, please call 021-63306968
Or send email to :sales@sunbowgroup.com
Hot Tags: magnetic shielding sheets, China magnetic shielding sheets manufacturers, suppliers, factory
Send Inquiry