Same magnetic cores, why do AI power supplies prefer nanocrystalline cores?
Nov 25, 2026
Same magnetic cores, why do AI power supplies prefer nanocrystalline cores?
Driven by the continuous expansion of AI computing infrastructure, the operating condition boundaries of server power supplies are being redefined. Compared with traditional telecom power supplies and ordinary industrial power supplies, AI power supplies must cope with heavy current surges, millisecond-scale load transients and high-temperature enclosed environments, while balancing high conversion efficiency, high power density and long-term continuous operational reliability. When these three constraints overlap, the magnetic material has to satisfy requirements on size, DC bias at high current and high-temperature stability simultaneously, rather than focusing solely on core loss. The old logic of "selecting materials by frequency" is no longer sufficient.
Another easily overlooked detail: the bus voltage has been raised from 48V to 800V. At the same power level, the current drops to approximately one-sixteenth, greatly cutting transmission losses. However, the voltage is not eliminated; instead, it is pushed closer to the chips. The post-stage DC-DC converters operate at lower voltages with higher currents, so the current stress on magnetic components rises rather than falls.

Preference 1: Common-mode inductors - the most mature application for nanocrystalline cores
A common-mode inductor does not act as a shielding can. It works through impedance division: the magnetic core presents high impedance at high frequencies to block common-mode current on the circuit path. In AI server power supplies, switching-frequency harmonics are dense and high-power, so this core has to meet three key requirements at once. First, sufficient impedance at high frequencies. Nanocrystalline materials feature high initial permeability and maintain considerable impedance from tens of kHz up to the MHz range, securing sufficient conducted emission margin. Second, resistance to saturation under high current. Three-phase common-mode inductors are subject to unbalanced currents. Once the core saturates, impedance plummets, rendering the inductor ineffective. The saturation flux density (Bs) of nanocrystalline material is around 1.2T, roughly three times that of power ferrites (0.38–0.42T at 100°C). Under the same flux design criteria, it supports higher operating flux density, enabling a smaller core size to fit high-density cabinet stacking. An engineering note: common-mode inductors are generally built without air gaps to preserve permeability, and their tolerance to unbalanced currents mainly relies on saturation flux density itself. This is why high Bs is hard to replace in this application.
Third, stable performance at hotspot temperatures. The loss curve of Mn-Zn ferrite is temperature-dependent, with an optimal operating window (roughly 80–100°C). Loss rises outside this range, and magnetic properties degrade rapidly near its Curie temperature of about 200°C.
Nanocrystalline material has a Curie temperature of around 560°C, with gentle property degradation at elevated temperatures. For cores placed close to heat sources, this advantage matters far more than datasheet figures suggest.
Preference 2: Medium-frequency isolation and PFC - a trade-off on size
10 kHz to 100 kHz is the operating frequency window for isolation stages and PFC inductors in many new-generation computing power supplies. Within this band, nanocrystalline material shows a typical specific core loss of around 20 W/kg at 20 kHz & 0.5T (value for uncut toroidal samples).
Combined with operating flux density above 1.2T, fewer winding turns and smaller cross-sectional area are required for the same power rating. Higher flux density shortens windings and reduces copper consumption - this economic consideration carries more weight amid high copper prices.
Dynamic bias performance is also critical. AI chip loads switch rapidly between training, inference and standby modes, so the magnetic core is continuously exposed to DC bias superimposed on AC flux. It should be noted that annealed nanocrystalline has an almost rectangular hysteresis loop and weak anti-bias performance without air gaps. With properly designed cut air gaps and winding structures, the linear range of the magnetic circuit is widened, and inductance attenuation under bias shock is moderated. Anti-DC-bias capability comes from magnetic circuit design, not only the ribbon material itself.

Where it is NOT preferred: clarifying application boundaries
No single material can cover all scenarios in AI power supplies. Nanocrystalline cores have clear application limits. Alloy powder cores remain the mainstream mass-production choice for TLVR coupled inductors, thanks to stable DC bias characteristics suitable for board-level VRM inductors; nanocrystalline and amorphous materials are still under evaluation for partial use cases. Mn-Zn ferrite retains an edge in core loss for high-frequency resonant links above 100 kHz. Magnetic powder cores offer better cost performance for cost-sensitive applications with steady loads. Silicon steel continues to dominate low-frequency and mains-frequency high-power applications.
Nanocrystalline material also has inherent drawbacks: higher unit cost, thin ribbon sensitive to mechanical stress. Stress can be introduced during cutting, winding, encapsulation and coating, shifting permeability and loss. It is a common challenge for engineers that samples perform well on bench tests yet deviate in performance after being assembled into inductors. Typical datasheet values are measured on standard coupons; re-testing is mandatory after cutting and gapping. Metal ribbons have much lower resistivity than ferrite, so parasitic capacitance between windings and the core is controlled entirely by insulating coating quality. Coating integrity directly affects high-frequency common-mode noise and voltage withstand capability.
Mass production: consistency matters as much as material performance
AI power supplies are mass-deployed equipment. A single unit contains multiple magnetic cores. Excessive parameter dispersion in one batch may lead to qualified prototype efficiency but declining mass yield. Therefore, more and more designs adopt multi-dimensional validation after material selection: core loss, permeability, bias characteristics and thermal cycling. Stable, repeatable test data supports mass design and avoids risks from relying only on spot prototype tests while ignoring parameter distribution.
The underlying rule is straightforward: nanocrystalline cores are chosen where size, DC bias and temperature requirements are all stringent. If only one constraint is demanding, ferrite or powder cores are usually more cost-effective. Instead of asking "which material is better" during component selection, first clarify the constraints of the specific location: operating frequency, flux swing, DC bias component, maximum hotspot temperature and cost target. Measured curves under target operating conditions, obtained before prototyping, are more reliable than any datasheet.