WebJul 28, 2022 · Abstract. Fe-based amorphous/nanocrystalline alloys exhibit excellent soft magnetic properties, including high saturation magnetic flux density ( B s ), high...
WebMay 1, 2021 · Fe-based amorphous alloy ribbons are synthesized via twin-roll strip casting. • As-spun ribbons have smooth appearance with more than 200 μm thickness. •...
WebJan 25, 2022 · Fe-based amorphous ribbons exhibit low core losses due to their ultra-thin thickness of 20–30 microns, higher electrical resistivity of 100–130 μΩ·cm and lack of...
WebAug 29, 2019 · The paper is devoted to the study of microstructural and magnetic properties of the Fe-based amorphous ribbons after interference pulsed laser heating. The...
WebFeb 1, 2021 · The Fe 78 Si 9 B 13 ribbons with the stress gradient possess a high magnetic susceptibility χ under a low external magnetic field (below Ha ). However, χ drops down...
WebSep 15, 2020 · The present study is focused on the microstructure evolution of Fe-based amorphous ribbons after pulsed laser interference heating and crystallization during...